Impact Resistance of Parylene C vs. Urethane and Epoxy
Impact resistance is high when the Parylene polymers are supported by testing panels.
MATERIAL | THICKNESS (Microns) | IMPACT RESISTANCE(kg-cm) |
Parylene C | 3 | >85 |
5 | >85 | |
8 | >85 | |
16 | >85 | |
30 | >85 | |
50 | >85 | |
73 | >85 | |
Urethane | 25 | 23 |
63 | 25 | |
125 | 51 | |
250 | 74 | |
375 | >85 | |
Epoxy | 125 | 35 |
250 | 81 | |
375 | >85 |